Název: | Rubber magnetic composites cross-linked with peroxide curing systems | ||||||||||
Autor: | Kruželák, Ján; Medlenová, Elena; Kvasničáková, Andrea; Dosoudil, Rastislav; Hudec, Ivan; Gořalík, Marek | ||||||||||
Typ dokumentu: | Recenzovaný odborný článek (English) | ||||||||||
Zdrojový dok.: | Polymer Science - Series B. 2019, vol. 61, issue 6, p. 865-873 | ||||||||||
ISSN: | 1560-0904 (Sherpa/RoMEO, JCR) | ||||||||||
Journal Impact
This chart shows the development of journal-level impact metrics in time
|
|||||||||||
DOI: | https://doi.org/10.1134/S1560090419060071 | ||||||||||
Abstrakt: | Abstract: Styrene–butadiene rubber and acrylonitrile–butadiene rubber as elastomer matrices were filled with barium ferrite in order to prepare rubber magnetic composites. For cross-linking of rubber compounds, peroxide curing systems consisting of dicumyl peroxide as curing agent and four types of low molecular weight organic compounds as co-agents were used. The work was focused on the investigation of different types of co-agents on the cross-linking, physical-mechanical and magnetic properties of the prepared composites. The results revealed that the type and amount of co-agent has no influence on magnetic characteristics of composites. On the other hand, cross-link density and physical-mechanical properties were significantly dependent on the composition of curing system. Co-agents contribute to the improvement of adhesion on the interphase filler-rubber. Considering the type of rubber matrix, higher values of tensile strength exhibited composites based on acrylonitrile–butadiene rubber. As magnetic filler and co-agents are polar materials, their compatibility with polar elastomers like acrylonitrile-butadiene rubber is much higher when compared to no-polar elastomers like styrene–butadiene rubber. © 2019, Pleiades Publishing, Ltd. | ||||||||||