Kontaktujte nás | Jazyk: čeština English
Název: | Swelling and rheological study of calcium phosphate filled bacterial cellulose-based hydrogel scaffold | ||||||||||
Autor: | Basu, Probal; Saha, Nabanita; Sáha, Petr | ||||||||||
Typ dokumentu: | Recenzovaný odborný článek (English) | ||||||||||
Zdrojový dok.: | Journal of Applied Polymer Science. 2019 | ||||||||||
ISSN: | 0021-8995 (Sherpa/RoMEO, JCR) | ||||||||||
Journal Impact
This chart shows the development of journal-level impact metrics in time
|
|||||||||||
DOI: | https://doi.org/10.1002/app.48522 | ||||||||||
Abstrakt: | This work focuses mainly about swelling and rheological properties of calcium phosphate filled bacterial cellulose (BC)-based hydrogel scaffolds. Calcium phosphate is incorporated in the form of hydroxyapatite (HA) and β-tricalcium phosphate (β-TCP) in different ratios, that is, 00:00, 10:90, 20:80, 40:60, 50:50, and 60:40. These scaffolds are also comprised with polyvinylpyrrolidone (PVP), poly(ethylene glycol), agar, and glycerin; designated as “BC-PVP” and “BC-PVP-β-TCP/HA.” All the hydrogel scaffolds are showing the notable viscoelastic property at 28 and 37 °C temperatures. The degree of swelling is found significant in BC-PVP-β-TCP/HA_50:50 scaffold and it is notably elastic at 37 °C after 5 min of swelling. However, after 60 min of swelling and at equilibrium swelling state, the elastic property of BC-PVP-β-TCP/HA_20:80 is revealed the highest. Considering the degree of swelling and rheological properties, the BC-PVP-β-TCP/HA_50:50 and BC-PVP-β-TCP/HA_20:80 hydrogel scaffolds found suitable for their application in bone tissue engineering or bone tissue regeneration. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019, 136, 48522. © 2019 Wiley Periodicals, Inc. | ||||||||||
Plný text: | https://onlinelibrary.wiley.com/doi/full/10.1002/app.48522 | ||||||||||
Zobrazit celý záznam |