Název: | Cross-linking epoxide resins with hydrolysates of chrome-tanned leather waste |
Autor: | Langmaier, Ferdinand; Mokrejš, Pavel; Kolomazník, Karel; Mládek, Milan; Karnas, Radoslav |
Typ dokumentu: | Recenzovaný odborný článek (English) |
Zdrojový dok.: | Journal of Thermal Analysis and Calorimetry. 2007, vol. 88, issue 3, p. 857-862 |
ISSN: | 1572-8943 (Sherpa/RoMEO, JCR) |
DOI: | https://doi.org/10.1007/s10973-005-7458-1 |
Abstrakt: | Differential scanning calorimetry was employed to investigate the reaction of diglycidyl ethers of bisphenol A (DGEBA) of mean molecular mass 348-480 Da, with collagen hydrolysate of chrome-tanned leather waste in a solvent-free environment. The reaction leads to biodegradable polymers that might facilitate recycling of plastic parts in products of the automotive and/or aeronautics industry provided with protective films on this basis. The reaction proceeds in a temperature interval of 205-220 degrees C, at temperatures approx. 30-40 degrees C below temperature of thermal degradation of collagen hydrolysate. The found value of reaction enthalpy, 519.19 J g(-1) (=101.24 kJ mol(-1) of epoxide groups) corresponds with currently found enthalpy values of the reaction of oxirane ring with amino groups. Reaction heat depends on the composition of reaction mixture (or on mass fraction of diglycidyl ethers in the reaction mixture) |
Plný text: | http://www.springerlink.com/content/707147g75k172gn3/ |
Zobrazit celý záznam |